Been using prusaslicers default PLA profile with issues and this is my first roll of PETG, so I just selected the corresponding profile for that.

It seems so be super stringy whenever there’s movement and when printing the bunny (in vase mode) there’s lots of holes in the model.

I’m not sure if this is an issue with calibration (didn’t do anything when switching from PLA) or if the filament is wet.

  • SymbioteSynapse@lemmy.world
    link
    fedilink
    English
    arrow-up
    8
    ·
    1 year ago

    Check for a partial clog. 80% of the time i get that consistency with petg, its because the nozzle is partially clogged. The other 20% is the ptfe tubing is shot. Usually it partially melts and causes underextrusion.

    Wet filament could be an issue too, but this is pretty extreme for wet filament.

  • blakcod@lemmy.ca
    link
    fedilink
    English
    arrow-up
    6
    ·
    1 year ago

    Do a temp tower. Find one hottest to coolest (260 to 220) and see where the sweet spot is. Going coolest to hottest could cause clogging.

    And when in doubt make sure you PETG is dry. Likes to pull in the moisture. Tell-a-tale is popping and hissing.

    Others: correct if I’m wrong but black PETG tends to be on the warmer side then other colours?

    • dack@lemmy.world
      link
      fedilink
      English
      arrow-up
      2
      ·
      1 year ago

      In my experience, moisture will cause excessive stringing in PETG long before it is saturated enough for popping/hissing.

    • drudoo@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      1
      ·
      1 year ago

      I did two temp towers: 260-225

      And

      280-235 Although my printer didn’t want to go above 260, so the first layers are all 260.

      • blakcod@lemmy.ca
        link
        fedilink
        English
        arrow-up
        2
        ·
        1 year ago

        Yikes! Are you sure you sliced the temp tower for PETG profile? (as others have inquired)

          • blakcod@lemmy.ca
            link
            fedilink
            English
            arrow-up
            1
            ·
            1 year ago

            Huge difference!

            Yeah I have Prusament Jet Black and 220/225 is the sweet spot for it on my setup.

            That’s a shame you have to do all of the replacements but looks to solve all sorts of things for you.

  • stealth_cookies@lemmy.ca
    link
    fedilink
    English
    arrow-up
    4
    ·
    1 year ago

    You sure you are using the PETG preset? The only time my PETG prints have looked like that is if I accidentally use the PLA preset and it under-extrudes because the temperatures aren’t high enough.

    • Hazdaz@lemmy.world
      link
      fedilink
      English
      arrow-up
      2
      ·
      1 year ago

      That’s literally the first thing I thought of as well. A few times that I’ve mistakenly tried printing with a PLA profile while PETG was in the printer. Doesn’t get hot enough and really struggles to push the material through (for obvious reasons).

      • poofy_cat@lemm.ee
        link
        fedilink
        English
        arrow-up
        1
        ·
        1 year ago

        This could be it, OP should check what the actual temperature says on the screen during printing.

  • bigredgiraffe@lemmy.world
    link
    fedilink
    English
    arrow-up
    3
    ·
    1 year ago

    My vote is a combo but it includes being wet, is this a new roll or if not how did you have it stored? I have found PETG to be much more finicky with moisture than PLA overall so if you have a way to dry it definitely try that and see what happens before trying to calibrate it.

      • bigredgiraffe@lemmy.world
        link
        fedilink
        English
        arrow-up
        2
        ·
        edit-2
        1 year ago

        I would try what that other person said, that’s a great idea!

        Anecdotally, I actually just got through half of a brand new roll today that I opened two days ago and it has been printing from a dry box and it started spattering from trapped moisture (you will find little chunks of plastic on your bed in past experience) so it’s in the dryer now haha.

        Hope it works out!

        ETA: I live in CO, USA and the humidity in the room where the printer is currently reads 70.4F/50% and the dry box reads 12% for reference, not much for it to soak up from the air.

  • sj_zero@lotide.fbxl.net
    link
    fedilink
    arrow-up
    2
    ·
    1 year ago

    I found petg to be a lot more challenging to print with than pla, but there’s a lot of really cool benefits to using petg like it’s more permanent and more flexible.

    I think the first thing to look at would be raising the temperature of your extruder. Seems like it isn’t really flowing a lot.

  • poofy_cat@lemm.ee
    link
    fedilink
    English
    arrow-up
    1
    ·
    edit-2
    1 year ago

    Aside from drying, here are some thoughts:

    Double-check the print temperature, PETG should be about 240-ish. Also the spiral vase mode may be the issue if your model isn’t designed for it. Also check your z offset, the first layer should be almost a flawless sheet… if not, stop the print and try again while live adjusting the z until it’s correct. Typically PETG doesn’t like to be squished down as much as PLA.

    • drudoo@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      1
      ·
      1 year ago

      Update: replaced the nozzle, heat block (heating element, sensor, PTFE) and fan duct. Did two new temp towers:

      Left tower is 235 (top) to 260 (layers labeled 280-260 are all 260). Right is 220-240.

      https://i.imgur.com/1MQkStE.jpg

      https://i.imgur.com/HDWq19A.jpg

      I definitely feel like 220 is the right temp for this.

      I’ll try the bunny again, the model is designed for vase mode, so it should work!

      • poofy_cat@lemm.ee
        link
        fedilink
        English
        arrow-up
        0
        ·
        1 year ago

        I had one weird roll of PETG that could only be printed at lower temperatures, so it’s possible. Still looks like the filament is wet to me… I recommend picking up a Sunlu S1 Plus when it drops under $40, I like being able to both dry the spool and print straight from the dryer (only takes a couple hours to re-absorb moisture).

        • drudoo@lemmy.worldOP
          link
          fedilink
          English
          arrow-up
          2
          ·
          1 year ago

          Dude! I just checked AliExpress for the Sunlu S1 Plus when I saw your message and was able to get one for $39 (shipped from Germany)! Thank you for that idea!